FUEL PROCESSING TECHNOLOGY
卷 110, 期 -, 页码 114-121出版社
ELSEVIER
DOI: 10.1016/j.fuproc.2012.12.003
关键词
Coal fly ash; Thermal activation; Alumina extraction; NaOH; Na2CO3
资金
- Shanxi Young Scientific and Technological Research Foundation [2011021008-2]
- International Scientific and Technological Cooperation of China [2011DFA90830]
- National Hi-Tech Research and Development Program of China (863 Program) [2011AA06A103]
The extraction of alumina from coal fly ash is a good direction for its value-added utilization. The presence of the inert matters with high degree of polymerization, such as mullite and other aluminosilicates, makes the reactivity of coal fly ash very poor. The activation of coal fly ash is necessary before its utilization. The thermal activation calcination with the addition of NaOH and Na2CO3 was carried out in this research. The results showed that the addition of NaOH and Na2CO3 improved the alumina extraction evidently. The maximum alumina extraction reached similar to 60% when calcination at 600-900 degrees C with the addition of NaOH and that could reach 82% at 900 degrees C with the addition of Na2CO3. Detailed analysis and characterization was carried out by using thermal gravimetric and differential scanning calorimetric analysis (TG-DSC) and X-ray diffraction (XRD). The results indicated that NaOH and Na2CO3 facilitated the decomposition of the polymeric phases. At lower temperatures (<600 degrees C), NaOH played a main role while Na2CO3 did at higher temperatures (> 700 degrees C). As a result, the mixed additives containing NaOH and Na2CO3 made alumina extraction attain 95% at 700 degrees C. (C) 2012 Published by Elsevier B.V.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据