4.7 Article

Effect of steam treatment on catalytic performance of HZSM-5 catalyst for ethanol dehydration to ethylene

期刊

FUEL PROCESSING TECHNOLOGY
卷 110, 期 -, 页码 73-78

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.fuproc.2012.11.004

关键词

HZSM-5; Ethanol dehydration; Dealumination; Steam treatment

向作者/读者索取更多资源

The effect of steam treatment on HZSM-5 catalysts was analyzed during ethanol dehydration to ethylene. The parent and the steam treated HZSM-5 catalysts were characterized by various techniques. The results showed that the steam treatment created new mesopores on HZSM-5 zeolites by increasing the treatment temperature, which resulted in the coexistence of micropores and mesopores. The total amount of acid sites and the Bronsted/Lewis ratios of HZSM-5 zeolites decreased after steam treatment, especially for the strong acid sites. The steam treated catalyst at 500 degrees C (HT500) exhibited excellent catalytic stability and good selectivity for ethanol dehydration to ethylene. The improvement in the catalytic stability can be attributed to lower acidity, lower ratio of B/L and newly created mesopores after steam treatment. The analyses of the coke depositions over the spent catalysts indicated that the HT500 catalyst contained less coke deposition than that over the parent HZSM-5 did. The newly created mesopores on catalyst during the steam treatment may accommodate part of coke deposition, suppressing the formation of coke deposition in its inherent micropores to some extent. (C) 2012 Published by Elsevier B.V.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据