The selective dehydration of glucose to hydroxymethylfurfural (HMF) in a biphasic medium (water/methylisobuthylketone) has been studied by using different catalysts based on mesoporous MCM-41 silica containing ZrO2. These catalysts have been: (a) MCM-41 silica doped with Zr in the synthesis step and activated at 550 and 750 degrees C, (b) this solid impregnated with sulphuric acid and activated at 750 degrees C, and (c) MCM-41 impregnated with zirconium sulphate and calcined at 750 degrees C. All these catalysts exhibit acidic properties (282-563 mu mol of NH3 desorbed g (1)) and high surface areas (359-635 m(2) g (1)), being active in the dehydration of glucose to HMF at 175 degrees C and 150 min of reaction time. Catalysts are quite selective, since only fructose and HMF were detected, whereas levulinic acid was absent. The most active catalyst was obtained after incorporation of zirconium into a MCM-41 silica in the synthesis gel (Zr-MCM-550), achieving a HMF yield of 23%. Moreover, the activity of the spent catalyst is fully recovered after calcination at 500 degrees C during 2 h. TOF values of these catalysts vary between 1.3 and 1.8 mmol of HMF g(-1) h(-1), being the catalytic performance well correlated with the acidity and textural characteristics of catalysts. (C) 2013 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据