Physical Entrapment of Hyaluronic Acid During Synthesis Results in Extended Release From Model Hydrogel and Silicone Hydrogel Contact Lens Materials

期刊

出版社

LIPPINCOTT WILLIAMS & WILKINS
DOI: 10.1097/ICL.0b013e318281ae06

关键词

Contact lens; Hydrogel; Hyaluronic acid; Lysozyme; Release; Wetting agent

资金

  1. Natural Sciences and Engineering Research Council of Canada (NSERC)
  2. 20/20 NSERC Ophthalmic Materials Network

向作者/读者索取更多资源

Objectives: This study was designed to assess the duration of hyaluronic acid (HA) release from model contact lens materials when HA was physically incorporated into the hydrogel during synthesis and to assess the effects of the HA release on lysozyme sorption. Methods: Model conventional and silicone hydrogel contact lens materials containing HA of various molecular weights as a releasable wetting agent were prepared. The HA was released into phosphate-buffered saline and MilliQ water, and the release was monitored using ultraviolet spectroscopy. Hyaluronic acid release was quantified by enzyme-linked immunosorbent assay. The effect of the releasable HA on lysozyme sorption to the materials was also analyzed using 125-I-labeled protein. Results: Hyaluronic acid loaded into the materials using this method could be released from conventional hydrogel materials for 21 days; the model silicone hydrogels showed release of more than 7 weeks. With one exception, the releasable HA decreased lysozyme sorption. Conclusions: Hyaluronic acid physically incorporated into contact lens materials during synthesis may therefore be released for extended periods of time of up to 7 weeks. Hyaluronic acid release leads to decreased protein adsorption in general. This method has potential for modification of conventional and silicone hydrogel lenses with releasable HA as a wetting agent.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据