4.4 Article

Partially bio-based thermoplastic elastomers by physical blending of poly(hydroxyalkanoate)s and poly(ethylene-co-vinyl acetate)

期刊

EXPRESS POLYMER LETTERS
卷 8, 期 7, 页码 517-527

出版社

BUDAPEST UNIV TECHNOL & ECON
DOI: 10.3144/expresspolymlett.2014.55

关键词

polymer blends and alloys; poly(hydroxybutyrate); poly(ethylene-co-vinyl acetate); miscibility; thermoplastic elastomer

资金

  1. National Natural Science Foundation of China [51303067, 51173072]
  2. Natural Science Foundation of Jiangsu Province [BK20130147]

向作者/读者索取更多资源

Partially bio-based thermoplastic elastomers (bio-TPE) were designed and prepared by physical blending a commercial grade poly(hydroxyalkanoate)s (PHBM, Metabolix) and poly(ethylene-co-vinyl acetate) (EVA). The PHBM is miscible with EVA90 which has a vinyl acetate (VA) content of 90 wt% while it is not miscible with EVA at low VA content (<= 70 wt%). The PHBM/EVA90 blends exhibit high tensile strength and typical thermoplastic elastomeric characteristics e.g. high elongation at break (> 800%), good strain-recovery (> 60%) and melt processability. The spherulite growth rate of PHBM decreases with increasing EVA90 content. Consequently, a large number of fine PHBM spherulites were formed in the blends. The spherulites act as physical crosslink-points leading to a thermoreversable network in the blends. Such network and elastic EVA90 molecules result in the thermoplastic and elastomeric characteristics of the PHBM/EVA90 blends.