4.7 Article Proceedings Paper

Modelling of ductile fracture initiation in strength mismatched welded joint

期刊

ENGINEERING FRACTURE MECHANICS
卷 75, 期 11, 页码 3499-3510

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.engfracmech.2007.04.026

关键词

ductile fracture initiation; welded joint; constraint effect; void volume fraction

向作者/读者索取更多资源

In this paper, the effect of strength mismatch and width of the welded joints oil the stress-strain distribution in the crack tip region has been discussed. The single-edge notched bend (SENB) specimens (precrack length a(0)/W= 0.32) were experimentally and numerically analysed. The model of local approach to fracture, proposed by Gurson, Tvergaard and Needleman, was used. High-strength low-alloyed (HSLA) steel was used as a base metal in quenched and tempered condition. The flux-cored arc-welding process in shielding gas was used. Two different fillers were selected to make over- and undermatched weld metal. The experimental analysis of fracture behaviour of the over- and undermatched welded joints was followed by numerical computations of void volume fraction in front of the crack tip. The critical void volume fraction, f(c), used in prediction of the crack growth initiation on the SENB specimen had been previously determined on a round smooth specimen. Three widths of weld metal were considered: 6,12 and 18 mm. A comparison of the crack tip opening displacement (CTOD) values corresponding to crack initiation in the SENB specimens is given, as determined both experimentally and using the GTN model. (C) 2007 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据