Nanostructuring of NiAl-Mo eutectic alloys by selective phase dissolution

期刊

ELECTROCHIMICA ACTA
卷 54, 期 25, 页码 6015-6021

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.electacta.2009.01.049

关键词

Nanostructures; Eutectic alloy; Selective dissolution; Electrochemical nanosystem technology

资金

  1. DAAD
  2. Deutsche Forschungsgemeinschaft [HA3118/4-3, SPP1165]

向作者/读者索取更多资源

A technique for the electrochemical structuring of directionally solidified NiAl-Mo eutectic by selective phase dissolution is presented. Local matrix dissolution at 200 mV SHE in I M HCl of pH 1 yielded the grid of Mo nanowires spanning along the central part of the sample. On the other hand, the dissolution of the fibrous minor phase while passivating the continuous NiAl matrix resulted in continuous nanopore arrays. Initially, mechanical polishing and electropolishing were employed to thin the samples. Etching time was optimized by plotting the etch time until hole formation as a function of initial sample thickness, along with plotting sample thickness versus etching time. As a next step, an investigation into the passivation behaviour of the NiAl was performed in order to determine the optimal potential for wire dissolution. A potential scan from 0 to 2500 mV SHE on a bulk sample of pure NiAl in an electrolyte of 0.1 M acetate buffer pH 6.0 indicated that a potential of 500 mV SHE, just below the breakdown potential would provide maximum driving force for wire dissolution process. Different parameters within the electrochemical system are varied in order to optimize the wire dissolution. The extent of wire dissolution is measured both quantitatively (total charge transfer) and qualitatively (optical and SEM imaging). (C) 2009 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据