4.6 Article

Effects of residual ethanol on the rate and degree of conversion of five experimental resins

期刊

DENTAL MATERIALS
卷 25, 期 5, 页码 621-628

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.dental.2008.11.005

关键词

Ethanol; DC; Methacrylate resins; Vapor pressure

资金

  1. National Institute of Dental and Craniofacial Research (NIDCR) [DE 014911]

向作者/读者索取更多资源

Objectives. This study examined the extent of ethanol retention in five comonomer blends of experimental methacrylate-based dental adhesives, containing (10, 20, or 30 wt.%) ethanol, after solvent evaporation, as well as observing the effect of residual ethanol and exposure duration on degree of conversion (DC). The null hypothesis that was tested was that residual, unevaporated ethanol has no effect on the rate or extent of DC of polymerized adhesive resins. Methods. A known mass of each mixture was placed in glass wells and evaporated for 60 s. The mass of the mixtures before and after evaporation was measured, allowing calculation of the gravimetric ethanol loss/retention. Results. The concentration of retained ethanol increased significantly with ethanol concentration (p<0.01): 1.1-1.9 mole/L for 10% ethanol/90% comonomers, 2.2-3.5 mole/L for 20% ethanol, and 2.6-3.7 mole/L for 30% ethanol/70% comonomers. As ethanol is evaporated from solvated comonomer mixtures, the molar concentration of comonomers increases, reducing the vapor pressure of the remaining ethanol. Thus, the fractional loss of ethanol solvent decreases as the comonomer concentration increases. The DC of 10, 20, and 30 wt.% ethanol blends increased with ethanol concentration in four of the five experimental resins (p < 0.05), increasing by 30-45% when 10 or 20 wt.% ethanol was added to neat resins, regardless of exposure duration. Depending on the resin system, inclusion of 30% ethanol lowered DC at 20 s but increased DC after 40-60 s of light exposure. Significance. Since 10 and 20 wt.% ethanol-resin blends increased the DC of solvated resins by 30-45% over neat resins, the test null hypothesis is rejected. Even with prolonged evaporation, 4-9% residual ethanol concentration can remain in 90/10 (wt./wt.) comonomer-ethanol mixtures. This is thought to be because comonomers lower the vapor pressure of ethanol. This amount of residual ethanol facilitates DC but lowers the rate of polymerization. (C) 2008 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据