In this paper, (Ca0.7Sr0.3)(Zr0.8Ti0.2)O-3 thin films were fabricated by RF-sputtering at various deposition temperatures from 300 degrees C to 700 degrees C to determine the optimal deposition condition. The XRD data confirmed the successful fabrication of crystalline CSZT thin films. Based on the dielectric properties of the fabricated thin films, the optimal deposition temperature was 700 degrees C, which resulted in a film with a relatively high dielectric constant and low dielectric loss (28.4 and 0.006) (at 1 MHz). Moreover, the CSZT thin film deposited at 700 degrees C showed stable dielectric properties at microwave frequencies. With increasing deposition temperature, the roughness of the CSZT thin film increased but the leakage current of the CSZT thin film decreased, simultaneously.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.2
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据