Model Fe-Cr and Fe-Cr-Ni alloys were reacted in Ar-CO2 and Ar-CO2-H2O gas mixtures at 650 C. Initially protective oxidation, due to Cr2O3 formation, was usually followed by a transition to rapid oxidation, associated with Fe-rich oxide nodule development. Nodule surface coverage and overall weight gains are modelled on the basis of continued nucleation of nodules, and their diffusion-controlled growth. In general, water vapour accelerated nucleation. Alloying with nickel decreased average nucleation rates, but austenitic alloys showed large variations in nucleation susceptibility with grain orientation. Slower nodule growth induced by high chromium and nickel levels counteracted the effects of frequent nucleation. (C) 2013 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据