Alloy; Copper; Tin; Electrochemical calculation; Polarization; Passive films
Corrosion of synthetic CuSn bronzes was electrochemically investigated on rotating disc electrode (RDE) in a buffered medium (pH = 6.8, deaerated 10(-2) mol L-1 Na2SO4 solution). Copper species diffusion coefficients through the patina for various tin-content bonzes were analyzed and provided information about its organization. A joined mass-transport and electronic transfer process controls the corrosion. A faster and more efficient passivation was observed with highest bronze tin-content. Also, copper species diffusion through the layer is independent of the tin content and few 10(-10) cm(2) s(-1). Such an order of magnitude indicates that corrosion products layer behaves like a gel. (C) 2013 Elsevier Ltd. All rights reserved.