As important structural materials for advanced power plants, the corrosion of 9-12% Cr ferritic-martensitic steels exposed to both high-temperature water and supercritical water (SCW) was studied using a variety of characterization techniques. Exposure temperature and time showed significant effects on the surface morphologies, oxide scale thickness, and oxide constituents. The steels approximately followed near-parabolic oxidation kinetics in the SCW conditions. The inner spinel layer was found to be porous with a size of tens of nanometers independent upon the exposure temperature and time. High temperature accelerated the formation of a large amount of pores in the outer magnetite layer. (C) 2010 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据