The degree of hydrogen embrittlement for several fastener grade steels has been determined. While microstructural alteration resulted in some improvement in resistance to hydrogen embrittlement, the overriding factor contributing to susceptibility of the steel was strength. The degree of susceptibility of the microstructures to hydrogen embrittlement, ranked in increasing order, is as follows: fine pearlite, bainite, tempered martensite. The effects of alloying were also assessed by comparing results from different fastener grade steels with similar microstructures. In most cases, the alloy chemistry had little effect, presumably due to trap saturation associated with this testing technique. (C) 2009 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据