In this investigation, Cr2O3 and MnCr2O4 were comparatively tested at 1050 degrees C in carbonaceous environment with varied oxygen partial pressures. MnCr2O4 exhibits much better resistance to carbonaceous attack than Cr2O3. The carburization rate of MnCr2O4 decreases sharply with increasing oxygen partial pressures. The oxygen partial pressures have less effect on the carburization resistance of Cr2O3. The increased resistance of MnCr2O4 to carburization is attributed to the dissolution of MnO into Mn-Cr-O spinel lattices with elevated oxygen partial pressures, which retards the decomposition and carburization of Mn-Cr-O spinel. The thermodynamic equations defining the carburization stability of MnCr2O4 and Cr2O3 are modified. (C) 2010 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据