Fire resistance of high-volume fly ash mortars with nanosilica addition

期刊

CONSTRUCTION AND BUILDING MATERIALS
卷 36, 期 -, 页码 779-786

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.conbuildmat.2012.05.028

关键词

Colloidal nanosilica; High-volume fly ash; High temperature; Strength; Microstructure

资金

  1. Universiti Kebangsaan Malaysia
  2. Ministry of Higher Learning Malaysia [FRGS/1/2011/TK/UKM/02/16]

向作者/读者索取更多资源

High-volume fly ash has been widely used in concrete to reduce the cost and environmental impact of producing cements. However, the effect of high temperature on cement-based materials containing fly ash and nanosilica has not been well characterized. In this study, cement was replaced by high-volume fly ash combined with colloidal nanosilica to produce high strength mortars with high residual strength after exposure to high temperatures of 400 degrees C and 700 degrees C. Heated and unheated specimens were subjected to flexural and compression tests. The samples were evaluated by scanning electron microscopy (SEM), X-ray diffraction (XRD) and thermogravimetric analysis (TGA) tests; and their porosity were determined using BET (Brunauer, Emmett, and Teller) technique to study the specimens' behavior after exposure to high temperatures. High strength mortars can be produced using nanosilica and fly ash with resultant high residual strength, as confirmed by the porosity, XRD and TGA tests results. (C) 2012 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据