Effect of delaying addition time of SMF superplasticizer on the physico-mechanical properties and durability of cement pastes

期刊

CONSTRUCTION AND BUILDING MATERIALS
卷 35, 期 -, 页码 261-269

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.conbuildmat.2012.02.068

关键词

Delaying addition time; Superplasticizer; Elevated temperature; Sulphate and chloride attack

向作者/读者索取更多资源

This research aimed to investigate the influence of delaying addition time of laboratory prepared sulphonate melamine formaldehyde (SMF) superplasticizer on the physico-mechanical characteristics and durability of cement pastes subjected to elevated temperature up to 800 degrees C, or immersed in 4% MgSO4 and 4% MgCl2. The compressive strength increases with delayed addition time at 7.5 min up to 90 days. The cement pastes containing 1.0 mass% SMF superplasticizer, with delayed addition time at 7.5 min, has highest compressive strength, bulk density and lower total porosity. The presence of SMF superplasticizer with delaying addition time process of mixing increases the compressive strength, bulk density and decreases the total porosity. These work together to produce a compact structure, inhibiting the chloride and sulphate ions penetration, hence the total sulphate and chloride contents decrease. (C) 2012 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据