4.7 Article

Failure analysis of (+/- 55 degrees)(3) filament wound composite pipes with an inclined surface crack under static internal pressure

期刊

COMPOSITE STRUCTURES
卷 92, 期 1, 页码 182-187

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.compstruct.2009.07.027

关键词

GRP pipe; Inclined surface crack; Burst strength; Internal pressure

资金

  1. Selcuk University

向作者/读者索取更多资源

This study conducts failure analysis of filament wound glass reinforced plastic (GRP) pipes made of E-glass/epoxy with an inclined surface crack under open-ended internal pressure. Test specimens are composed of six antisymmetric layers with (+/- 55 degrees)(3) winding angles. Tests have been performed at seven different crack angles: 0 degrees, 15 degrees, 30 degrees, 60 degrees, 45 degrees, 75 degrees, and 90 degrees, with crack-to-thickness ratio of a/t = 0.50. The burst strengths of the specimens were determined, and the dependence of the burst strength on the crack angle was examined. Published by Elsevier Ltd.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据