Centrifugal pumps used in the lignite mines encounter erosive wear problems, leading to a disastrous failure of the pump casings. This paper attempts to evaluate the erosive wear resistance of Ni-Hard 4, high-chromium iron, and Cast CD4MCu duplex stainless steel (DSS), for mining conditions. The prepared test coupons were subjected to an erosion test by varying the impingement velocity and the angle of impingement, under two different pH conditions of 3 and 7, which pertained to the mining conditions. XRD analysis was carried out to confirm the phases present in the alloy. The eroded surface was subjected to SEM analysis to identify the erosion mechanisms. The surface degradation of Ni-Hard 4 and high-chromium iron came from a low-angle abrasion with a grooving and plowing mechanism at a low angle of impingement. At normal impingement, deep indentations resulted in lips and crater formations, leading to degradation of the surface in a brittle manner. A combined extrusion-forging mechanism is observed in the CD4MCu DSS surface at all the impingement angles.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据