4.3 Article Proceedings Paper

Degradation of polyimide and polyethyleneterephtalate irradiated with 150 and 200 keV Ar+ ions, studied by RBS and ERD techniques

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/S0168-583X(99)00951-9

关键词

polymers; ion implantation; degradation; RBS; ERD

向作者/读者索取更多资源

Polyimide (Upilex, PI) and polyethyleneterephtalate (Mylar, PET) were irradiated with 200 and 150 keV Ar+ ions respectively to different fluences and the depth profiles of hydrogen and oxygen atoms in polymer surface layer were determined using standard Rutherford backscattering (RBS) and elastic recoil detection (ERD) techniques. Significant hydrogen and oxygen depletion is observed at the ion fluences above 1 x 10(14) cm(-2). Above 5 x 10(15) cm(-2) a saturated state is achieved when another fluence increase does not result in significant changes of the H and O profile shape. At higher fluences the H and O depth profiles are rather flat with no local minima. This finding indicates only minor role of nuclear stopping in production of volatile degradation products. (C) 2000 Elsevier Science B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据