Thermal degradation studies of some aliphatic polyamides using hyphenated techniques (TG-MS, TG-FTIR)

期刊

JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY
卷 59, 期 1-2, 页码 385-394

出版社

KLUWER ACADEMIC PUBL
DOI: 10.1023/A:1010177105297

关键词

polyamides; TA-FTIR; TA-MS; thermal degradation

向作者/读者索取更多资源

The thermal degradation of the aliphatic polyamides 6 and 66 was investigated by means of the combined techniques TA-MS and TA-FTIR. The analyses were performed in three different devices. Sample mass ranged from 13 mg to 1 g and heating rates of 2.6 and 10 K min(-1) were used in both air and nitrogen atmospheres. The most important decomposition products were caprolactam for PA 6 and cyclopentanone for PA 66. Evolution of NH3 and HCN was registered. The findings of the two hyphenated techniques led to the same results and complemented each other well. The evolved products were captured and analyzed off-line by GC/MS for further confirmation of results.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据