Relaxer ferroelectric single crystals Pb((Mg1/3Nb2/3)(1-x)Ti-x)O-3 (PMNT 100(1-x)/100x) were grown directly from melt by a modified Bridgman technique. The segregation during the growth of PMNT single crystals was studied by means of differential thermal analysis (TGA), thermogravimetric analysis (DTA), X-ray diffraction (XRD) and X-ray fluorescence analyzer (XRFA). The results show that PbTiO3 content increases throughout the crystal growth. The segregation coefficient is about 0.95 during the growth of PMNT 76/24 directly from melt. Therefore, the electric properties of PMNT single crystals vary even in the same boule. It was demonstrated that the homogeneity of PMNT single crystals can be improved by optimizing growth parameters, but it cannot be eliminated because of the effect of segregation during the crystal growth. We have recently improved the growth process of the modified Bridgman technique to increase the homogeneity of the crystals. Good-quality single crystals with a boule size of more than phi 40 x 80 mm or 30 x 30 x 1 mm plates have been achieved. For PMNT 67/33 crystals, their coupling factors are k(33) approximate to 94% for the longitudinal mode, k'(33) approximate to 86% for the beam mode, and k(t) approximate to 62% for the thickness mode, and they have the piezoelectric constant d(33) = 1500-3000 pC/N, and dielectric. constant epsilon (33)/epsilon (0) = 3500-5500.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

3.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据