4.5 Article

Effect of drying method on mesoporosity of resorcinol-formaldehyde drygel and carbon gel

期刊

DRYING TECHNOLOGY
卷 19, 期 7, 页码 1319-1333

出版社

MARCEL DEKKER INC
DOI: 10.1081/DRT-100105291

关键词

BET surface area; freeze drying; hot air drying; microwave drying; pore size distribution; pyrolysis; sol-gel polycondensation

向作者/读者索取更多资源

Resorcinol-formaldehyde hydrogels were synthesized by sol-gel polycondensation of resorcinol with formaldehyde in a slightly basic aqueous solution. RF cryogels, RF xerogels, and RF xerogels (MW gets) were respectively prepared from RF hydrogels by freeze drying, hot air drying, and microwave drying. Carbon cryogels, carbon xerogels and carbon MW gels were subsequently obtained by pyrolyzing RF drygels in an inert atmosphere. Freeze drying and microwave drying were effective to prepare mesoporous RF drygels and carbon gels. RF cryogels and carbon cryogels showed high mesoporosity over wide ranges of the molar ratio of resorcinol to catalyst (R/C) and the ratio of resorcinol to water (R/W) used in sol-gel polycondensation, Although RF xerogels had a few mesopores, carbon xerogels had no mesopores. RF MW gels and carbon MW gels showed mesoporosity if appropriate values of R/C and R/W were selected.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据