wool fabric; keratin fibers; glow discharge; contact angle; ageing; chitosan; SEM; Herbig sac

向作者/读者索取更多资源

The influence of the gas type, air or nitrogen, and the treatment time in an RF glow discharge treatment on the shrink resistance properties of knitted wool fabric and wetting properties of keratin fibres were studied. Wetting properties were determined by means of contact angle measurements on single keratin fibres. This method allows measuring accurately the influence of the plasma gas type and treatment time on fibre hydrophilicity, and its modification with the time elapsed after plasma treatment. The modification of the surface properties should be taken into account, especially, when a biopolymer after-treatment is applied to achieve wool shrink resistance. Surface chemical changes were studied by means of XPS. Topographical changes in the wool fibre surface were observed by scanning electron microscopy (SEM) and surface damage was evaluated by means of the Herbig sac formation. Both air and nitrogen plasma treatments impart shrink resistance to wool fabric and hydrophilic properties to the keratin fibres. Even short exposure times are found to be enough to decrease drastically the advancing water contact angle and, therefore, to increase the shrink resistance effect. Slight differences were observed between the air and nitrogen plasma treatments. The time elapsed after the plasma treatment promotes an increase of the advancing contact angle and a decrease of chitosan adsorption. The plasma treatments studied here modify chemically the epicuticle but it is not removed.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据