Titanium diboride nanoparticles were prepared from TTIP and boron oxide using a sol-gel method followed by mechano-chemical reduction in the presence of aluminum. Optimum weight ratio of B2O3:TTIP:2-propanol was 1:3:60. The XRD results revealed that mechano-chemical reduction of the zerogel by aluminum had led to the formation of TiB2 and Al2O3 phases after 15 hours of milling. The XRD results confirmed complete removal of Al2O3 via leaching the milled sample in 10 M NaOH at 150 degrees C. SEM and TEM studies showed that the mean particle size of the synthesized TiB2 is less than 30 nm. The densification experiments were carried out using hot pressing and pressureless sintering. The binderless densification of monolithic TiB2 up to 92% theoretical density was achieved by hot pressing at 1700 degrees C for 2 h in vacuum. The hot pressed TiB2 exhibits high Vickers hardness (25.9 GPa) and relative high fracture toughness (5.7 MPa.m(1/2)). In the pressureless sintering route, a maximum density of 82.3% NI, is achieved after sintering at 1900 degrees C for 2 h in vacuum. (C) 2014 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据