Tribological behaviour of zirconia-toughened alumina (ZTA) with different metal oxide additives was studied. Solid oxide lubricants (MOx; M = Cu, Ti, Mg, Zn, Mn) were added in small quantities (similar to 8-11 wt%) to provide a self-lubrication action and thereby to decrease the coefficient of dry friction. Dry mixed ceramic composites powders were compacted and pressureless sintered at different temperatures. Densification studies show that near full densities (>97%) were obtained for ZTA ceramic containing both TiO2-CuO and TiO2-MnO2 at 1450 degrees C. Phase and qualitative compositional analysis was done using X-ray diffraction (XRD) and energy-dispersive spectroscopy (EDS). Tribological behaviour of the various ZTA composites was tested by dry sliding the different specimens against SiC abrasive grit paper at a load of 50 N. The lowest specific wear rate of 9.2 x 10(-5) mm(3)/N m and coefficient of friction of 0.35 were observed for the ZTA ceramic composite with TiO2-MnO2. The basic wear mechanisms were abrasion and grain pullout as corroborated from scanning electron microscopy (SEM) images. (C) 2008 Published by Elsevier Ltd and Techna Group S.r.l.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据