To ensure the safety of metals and alloys intended for food contact, a new European test protocol (CoE protocol) using citric acid as a food simulant was published in 2013. This study investigated the influence of citric acid and exposure conditions on the metal release from an austenitic manganese stainless steel (AISI 201). Exposures in 5 g/L citric acid resulted in significantly lower metal releases compared with specific release limits set by the CoE protocol. 5 g/L (0.3 vol%) citric acid was more aggressive than 3 vol% acetic acid (Italian protocol) due to higher metal complexation. Studies on abraded surfaces revealed that most metals were released during the first 0.5 h of exposure due to surface passivation. Surface abrasion, increased temperature (40-100 degrees C), increased surface area to solution volume ratio (0.25-2 cm(2)/mL) and increased citric acid concentration (0-21 g/L) all resulted in increased released metal quantities. (C) 2014 The Authors. Published by Elsevier Ltd.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据