4.7 Article

Degrees of polymerization (DP) and DP distribution of cellouronic acids prepared from alkali-treated celluloses and ball-milled native celluloses by TEMPO-mediated oxidation

期刊

CELLULOSE
卷 16, 期 1, 页码 117-127

出版社

SPRINGER
DOI: 10.1007/s10570-008-9245-1

关键词

TEMPO; Cellouronate; Cellouronic acid; Ball-milling; Mercerized cellulose; Regenerated cellulose; Molecular mass; SEC-MALLS; LODP

资金

  1. Japan Society for the Promotion of Science (JSPS) [r 15658052]

向作者/读者索取更多资源

Various cellulose II samples, ball-milled native celluloses and ball-milled wood saw dust were subjected to 2,2,6,6-tetramethypyperidine-1-oxyl radical (TEMPO)-mediated oxidation to prepare cellouronic acid Na salts (CUAs). The TEMPO-oxidized products obtained were analyzed by C-13-NMR and size-exclusion chromatography (SEC). When the cellulose II samples with degrees of polymerization (DP) of 220-680 were used as the starting materials, the CUAs obtained had weight-average DP (DPw) values of only 38-79. Thus, significant depolymerization occurs on cellulose chains during the TEMPO-mediated oxidation. These DP values of CUAs correspond to the cellulose II crystal sizes along the chain direction in the original cellulose II samples, but not necessarily to their leveling-off DP values. CUAs can be obtained also from ball-milled native celluloses in good yields by TEMPO-mediated oxidation, although their DPw values are lower than about 80. On the other hand, CUA with DPw of about 170 was obtained from ball-milled wood saw dust.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据