4.7 Article

Solvent debinding mechanism for alumina injection molded compacts with water-soluble binders

期刊

CERAMICS INTERNATIONAL
卷 29, 期 7, 页码 745-756

出版社

ELSEVIER SCI LTD
DOI: 10.1016/S0272-8842(02)00226-2

关键词

injection molding; porosity; Al2O3; solvent debinding

向作者/读者索取更多资源

The solvent debinding process has been widely accepted in the ceramic injection molding (CIM) industry process due to its short debinding cycle. However, the organic solvents most adopted in solvent debinding now are flammable, carcinogenic and not environmentally acceptable. For eliminating the use of unsound solvents, water-soluble polyethylene glycol (PEG) is used in this study to modify the pattern of debinding in CIM. The purpose of the investigation was to examine the binder behavior during solvent debinding based on water extraction for a multi-component PEG binder system. Based on the in situ evaluation results of dimensional variations, mercury intrusion data and scanning electron microscope (SEM) observations, possible solvent debinding mechanism for alumina injection molded compacts with water-soluble binders is proposed. (C) 2003 Elsevier Ltd and Techna S.r.l. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据