Density loss and respiration rates in coarse woody debris of Pinus radiata, Eucalyptus regnans and Eucalyptus maculata

期刊

SOIL BIOLOGY & BIOCHEMISTRY
卷 35, 期 1, 页码 177-186

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/S0038-0717(02)00255-9

关键词

coarse woody debris; wood density; wood respiration; decomposition

向作者/读者索取更多资源

This study compared field and laboratory decomposition rates of coarse woody debris (CWD) (> 10 cm diameter) from three tree species: Pinus radiata, Eucalyptus regnans, and Eucalyptus maculata. For this purpose, the density loss of logs on the ground sampled from chronosequences of sites following harvesting was determined using the water replacement technique. P. radiata logs were sampled 1, 2.5, 6, and 9 years following harvesting, and logs of E. regnans and E. maculata were collected from sites that were harvested 1, 3.5, 6.5, and 12 and 1.5, 6.5, and 11.5 years ago, respectively. In addition, the ON ratio of wood was determined and current respiration rates of logs from these different age classes were measured through laboratory incubation. The times for loss of 95% of material (t(0.95)) determined from density loss for these species were 24 years for P. radiata, 43 years for E. regnans, and 62 years for E. maculata. The decomposition rates of CWD derived from laboratory respiration were 6.1, 5.9 and 11.9 times higher than the decay rates from density loss in P. radiata, E. regnans, and E. maculata, respectively. This points to severe constraints of decomposition through adverse conditions in the field. The changes in respiration rates and C/N ratio with age of decaying logs indicated that the single component, negative exponential decay model could be applied satisfactorily only to P. radiata. In the case of the eucalypt species, substrate quality (expressed through respiration rates) declined in the oldest samples. This may be explained by the loss of rapidly decomposing sapwood and the retention of more decay-resistant heartwood. In these cases, a two-component model will be more suitable to describe the density loss of decaying wood. (C) 2003.Elsevier Science Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据