Protection of silicon nitride ceramics against corrosion in acidic aqueous solutions by enforced internal passivation

期刊

CERAMICS INTERNATIONAL
卷 30, 期 2, 页码 267-271

出版社

ELSEVIER SCI LTD
DOI: 10.1016/S0272-8842(03)00098-1

关键词

grain boundary; corrosion; Si3N4; structural applications

向作者/读者索取更多资源

Silicon nitride ceramics with Y2O3 and Al2O3 as sintering additives were corroded in 1 N sulphuric acid at 90degreesC. Any classical corrosion rate model cannot describe the overall kinetics of the corrosion process successfully. At longer corrosions times, a kinetic break occurs, after which slow linear corrosion kinetics prevail. The passivation is due to the formation of a defective silica sublayer in the corrosion zone. We show that it is possible to enforce this passivation long before it would occur naturally by a simple hot drying (150degreesC) procedure after a critical time. As consequence the total mass loss decreases by a factor of 2-3. (C) 2003 Elsevier Ltd and Techna S.r.l. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据