A green method is reported to effectively and rapidly reduce graphene oxide to graphene with zinc powder at room temperature. The reduction is carried out by mixing graphene oxide and zinc powder in solution under ultrasonication. The reduction is complete within 1 min. The weight of the Zn powder should be at least as twice as that of graphene oxide to complete the reduction. The reduction of graphene oxide is confirmed by FTIR, UV-Vis absorption spectroscopy and Raman spectroscopy. The carbon/oxygen atomic ratio has increased from 2.58 to 33.5 after the reduction as determined by X-ray photoelectron spectroscopy. The reduced graphene oxide can have a conductivity of 15,000 S/m. It also has good thermal stability with the weight loss at 590 degrees C in air. The reduced graphene oxide can be readily re-dispersed into solutions of various surfactants. (C) 2011 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据