4.7 Article

Dissolution of mechanically milled chitin in high temperature water

期刊

CARBOHYDRATE POLYMERS
卷 106, 期 -, 页码 172-178

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.carbpol.2014.02.009

关键词

Chitin; High temperature water; Mechanical milling; Reaction mechanism

资金

  1. Global COE

向作者/读者索取更多资源

Chitin is high in crystallinity in its natural form and does not dissolve into high temperature water (HTW), which often leads to decomposition reactions such as hydrolysis, deacetylation and dehydration when hydrothermally processed. In this work, we investigated the reactions of mechanically milled chitin in HTW. Mechanical milling pretreatment combined with HTW treatment improved the liquefaction of chitin giving a maximum water soluble fraction of 80%, where the untreated chitin was 55%. The reaction mechanism of the milled and raw chitin in HTW was shown to be different. For milled chitin, the dissolution of chitin occurred during the heating period to supercritical water conditions (400 degrees C) at short reaction times (1 min). Extended reaction time (10 min) led to decomposition products and aromatic char formation. For raw chitin, the dissolution of chitin in HTW did not occur, due to its high crystallinity, so that liquefaction proceeded via decomposition reactions. (C) 2014 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据