4.0 Article

Room-temperature solid-state sodium/sulfur battery

期刊

ELECTROCHEMICAL AND SOLID STATE LETTERS
卷 9, 期 3, 页码 A123-A125

出版社

ELECTROCHEMICAL SOC INC
DOI: 10.1149/1.2164607

关键词

-

向作者/读者索取更多资源

Solid-state sodium/sulfur batteries using polyvinylidene-fluoride-hexafluoropropene (PVDF) polymer electrolyte were prepared and tested at room temperature. Solid sodium/sulfur batteries may be composed of solid-composite-type sulfur electrodes, sodium metal electrodes, and PVDF gel polymer electrolyte. The PVDF gel polymer electrolyte with tetraglyme plasticizer and NaCF3SO3 salt had a high sodium ion conductivity of 5.1 x 10(-4) S cm(-1) at 25 degrees C. During the first discharge, the sodium/sulfur battery showed two plateau potentials of 2.27 and 1.73 V, respectively. The first discharge capacity was 489 mAh/g sulfur at room temperature, which was similar to the high temperature battery. The discharge capacity drastically decreased by repeated charge-discharge cycling, and remained at 40 mAh/g after 20 cycles. (c) 2006 The Electrochemical Society.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.0
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据