It is important to develop the production and utilization technology of highly reactive coke in order to improve the efficiency of blast furnace reactions. In this study, the characteristics of catalyst-coated highly reactive coke produced by the 'post-addition of catalyst to coke' method were investigated. First, the catalytic effect of Fe and Ca on graphite and deashed coke during the C-CO2 reaction was investigated. Fe and Ca addition increased the reaction rate and decreased the reaction beginning temperature. Second, the reaction rate of Fe or Ca coated coke was kept high until the weight loss reached 10%. This means that a high catalytic effect is maintained in the thermal reserve zone of the blast furnace. Furthermore, it was found that 70% of the catalyst coated on the coke surface remains after drop impacts. It is expected that the loss of catalyst during coke handling and transportation is small. Catalyst-coated highly reactive coke is promising for improving the efficiency of blast furnace reactions.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据