4.7 Article

Impact of zeta potential of early cement hydration phases on superplasticizer adsorption

期刊

CEMENT AND CONCRETE RESEARCH
卷 37, 期 4, 页码 537-542

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.cemconres.2007.01.007

关键词

adsorption; admixture; ettringite; monosulfate; zeta potential

向作者/读者索取更多资源

The zeta potential of early hydration products of cement was found to be a key factor for superplasticizer adsorption. A highly positive zeta potential results in a strong superplasticizer adsorption whereas a negative zeta potential does not allow adsorption. Synthetic ettringite precipitated from solution shows a highly positive zeta potential, hence it adsorbs great amounts of negatively charged superplasticizer. Monosulfate (AF(m)) has a less positive zeta potential. Therefore, it adsorbs smaller amounts of superplasticizers. For syngenite, portlandite and gypsum, the zeta potential is around zero or negative. These phases do not adsorb superplasticizers. Consequently, a hydrating cement grain is best represented by a mosaic structure, with superplasticizer molecules mainly adsorbed on ettringite and some on monosulfate and C-S-H nucleated at surface. (c) 2007 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据