Sodium deficiency in Na0.5Bi0.5TiO3

期刊

JOURNAL OF MATERIALS CHEMISTRY
卷 17, 期 2, 页码 185-192

出版社

ROYAL SOC CHEMISTRY
DOI: 10.1039/b609606a

关键词

-

向作者/读者索取更多资源

The mechanism of solid-state synthesis for Na0.5Bi0.5TiO3 was investigated using X-ray powder diffraction, scanning electron microscopy and wavelength-dispersive X-ray spectroscopy. The results showed that a Na0.5-xBi0.5TiO3-x/2 homogeneity region, with Na0.5Bi0.5TiO3 and Na0.47Bi0.5TiO3-delta as the end-members (0 <= x <= 0.03), exists in the Na2O - Bi2O3 - TiO2 system. The formation of any member from the homogeneity region starts with the formation of the deficient end-member, i.e., Na0.47Bi0.5TiO3-delta. However, the reaction continues toward a nominal composition when a sufficiently high temperature and/or a long firing time are used. The conversion of the latter reaction may be followed by the observation of the crystal symmetry, which changes from the cubic-like toward the rhombohedral as the reaction proceeds from Na0.47Bi0.5TiO3-delta to Na0.5Bi0.5TiO3. Differences in the dielectric, ferroelectric and piezoelectric properties were observed for the samples from the homogeneity region, and these can be related to the stoichiometry variation along the homogeneity region and thus to the variation in the vacancy concentration. The most striking difference is the change in the piezoelectric constant d(33), which increases from 82 pC N-1 to 97 pC N-1 as the composition of the ceramics changes from Na0.5Bi0.5TiO3 to Na0.47Bi0.5TiO3-delta.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据