The current study aims to investigate the behaviour of high-volume fly ash (HVFA) concrete blended with ground granulated blast-furnace slag (shortened as slag) under the effect of elevated temperatures. For this reason, cement has been partially replaced with a Class F fly ash (FA) at a level of 70% to produce HVFA concrete (F70). F70 was modified by partially replacing FA with slag at levels of 10% (F60G10) and 20% (F50G20), by weight. All HVFA concrete types were compared to the neat Portland cement (PC) concrete (F0). After curing, the specimens were exposed to elevated temperatures ranging from 400 degrees C to 1000 degrees C with an interval of 200 degrees C. Weight and compressive strength before and after being exposed to elevated temperatures have been thoroughly explored. The various decomposition phases formed were identified using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results indicated higher relative strength of all HVFA concrete types. F70 exhibited the highest relative strength among all studied mixtures. The incorporation of slag showed negative effect on HVFA concrete before and after different heat treatments. The inclusion of slag caused a reduction in the residual compressive strength of F70 approximately ranging from 14% to 21%. (C) 2015 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据