The performance of two pretreatment methods, sulfite pretreatment to overcome recalcitrance of lignocellulose (SPORL) and dilute acid (DA), was compared in pretreating softwood (spruce) for fuel ethanol production at 180 degrees C for 30 min with a sulfuric acid loading of 5% on oven-dry wood and a 5:1 liquor-to-wood ratio. SPORL was supplemented with 9% sodium sulfite (w/w of wood). The recoveries of total saccharides (hexoses and pentoses) were 87.9% (SPORL) and 56.7% (DA), while those of cellulose were 92.5% (SPORL) and 77.7% (DA). The total of known inhibitors (furfural, 5-hydroxymethylfurfural, and formic, acetic and levulinic acids) formed in SPORL were only 35% of those formed in DA pretreatment. SPORL pretreatment dissolved approximately 32% of the lignin as lignosulfonate, which is a potential high-value co-product. With an enzyme loading of 15 FPU (filter paper units) per gram of cellulose, the cellulose-to-glucose conversion yields were 91% at 24 h for the SPORL substrate and 55% at 48 h for the DA substrate, respectively. (C) 2009 Elsevier Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据