4.2 Article

Fabrication and evaluation of poly(epsilon-caprolactone)/silk fibroin blend nanofibrous scaffold

期刊

BIOPOLYMERS
卷 97, 期 5, 页码 265-275

出版社

WILEY-BLACKWELL
DOI: 10.1002/bip.22016

关键词

poly(?-caprolactone); silk fibroin; scaffold; electrospinning; nanofiber

资金

  1. Korea Science and Engineering Foundation (KOSEF) [R11-2005-065]
  2. Rural Development Administration, Republic of Korea [2008FTH010102001]
  3. National Research Foundation of Korea [2008-0057394] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

向作者/读者索取更多资源

In this study we investigated the blend electrospinning of poly(epsilon-caprolactone) (PCL) and silk fibroin (SF) to improve the biodegradability and biocompatibility of PCL-based nanofibrous scaffolds. Optimal conditions to fabricate PCL/SF (50/50) blend nanofiber were established for electrospinning using formic acid as a cosolvent and three-dimensional (3D) PCL/SF blend nanofibrous scaffolds were prepared by a modified electrospinning process using methanol coagulation bath. The physical properties of 2D PCL/SF blend nanofiber mats and 3D highly porous blend nanofibrous scaffolds were measured and compared. To evaluate cytocompatibility of the 3D blend scaffolds as compared to 3D PCL nanofibrous scaffold, normal human dermal fibroblasts were cultured. It is concluded that biodegradability and cytocompatibility could be improved for the 3D highly porous PCL/SF (50/50) blend nanofibrous scaffold prepared by blending PCL with SF in electrospinning. In addition to the blending of PCL and SF, the 3D structure and high porosity of electrospun nanofiber assemblies may also be important factors for enhancing the performance of scaffolds. (c) 2011 Wiley Periodicals, Inc. Biopolymers 97: 265275, 2012.