期刊
BIOMATERIALS
卷 30, 期 27, 页码 4601-4609出版社
ELSEVIER SCI LTD
DOI: 10.1016/j.biomaterials.2009.05.007
关键词
Cell adhesion; Cell viability; Hydrogel; PolyHEMA; Porosity
资金
- EU [LSHM-CT-2007-037862]
- Academy of Sciences of the Czech Republic [KAN200520804]
Modifications of poly(2-hydroxyethyl methacrylate) (PHEMA) with cholesterol and laminin have been developed to design scaffolds that promote cell-surface interaction. Cholesterol-modified superporous PHEMA scaffolds have been prepared by the bulk radical copolymerization of 2-hydroxyethyl methacrylate (HEMA), cholesterol methacrylate (CHLMA) and the cross-linking agent ethylene dimethacrylate (EDMA) in the presence of ammonium oxalate crystals to introduce interconnected superpores in the matrix. With the aim of immobilizing laminin (LN), carboxyl groups were also introduced to the scaffold by the copolymerization of the above monomers with 2-[(methoxycarbonyl)methoxy]ethyl methacrylate (MCMEMA). Subsequently, the MCMEMA moiety in the resulting hydrogel was hydrolyzed to 12(methacryloyloxy)ethoxy]acetic acid (MOEAA), and laminin was immobilized via carbodiimide and N-hydroxysulfosuccinimide chemistry. The attachment, viability and morphology of mesenchymal stem cells (MSCs) were evaluated on both nonporous and superporous laminin-modified as well as laminin-unmodified PHEMA and poly(2-hydroxyethyl methacrylate-co-cholesterol methacrylate) P(HEMA-CHLMA) hydrogels. Neat PHEMA and laminin-modified PHEMA (LN-PHEMA) scaffolds facilitated MSC attachment, but did not support cell spreading and proliferation: the viability of the attached cells decreased with time of cultivation. In contrast, MSCs spread and proliferated on P(HEMA-CHLMA) and LN-P(HEMA-CHLMA) hydrogels. (C) 2009 Elsevier Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据