Formation of peptide impurities in polyester matrices during implant manufacturing

出版社

ELSEVIER
DOI: 10.1016/S0939-6411(00)00066-7

关键词

peptide; polylactic acid; melt-processing; impurity; vapreotide

向作者/读者索取更多资源

Most peptides are susceptible, in vivo, to proteolytic degradation, and it is difficult to formulate and to deliver them without loss of biological activity. In addition, it is often desirable to release them continuously and at a controlled rate over a period of weeks or months. For these reasons, a controlled release system is suitable. Poly(lactic acid) (PLA) is a biocompatible and biodegradable material that can be used for many applications, including the design of injectable controlled release systems for pharmaceutical agents. Development of these delivery systems presents challenges in the assessment of stability, specially for peptide drugs. By means of an extrusion method, long-acting poly(lactic acid) implants containing vapreotide, a somatostatin analogue, were prepared. The nature of the main degradation product obtained after implant manufacturing was elucidated. It was found that the main peptide impurity was a lactoyl lactyl-vapreotide conjugate. Because lactide are found in small quantities in most commercially available PLA, the influence of residual lactide in the polymeric matrix, on the formation of peptide impurities during manufacturing, was specially investigated. This work demonstrates that the degree of purity of the carrier is of great importance with regard to the formation of peptide impurities. (C) 2000 Elsevier Science B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据