Effect of grinding on synthesis of MgAl2O4 spinel from a powder mixture of Mg(OH)2 and Al(OH)3

期刊

POWDER TECHNOLOGY
卷 113, 期 1-2, 页码 109-113

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/S0032-5910(00)00208-4

关键词

MgAl2O4 spinel; mechano chemical treatment; planetary ball mill; magnesium hydroxide; gibbsite

向作者/读者索取更多资源

Dry grinding of the powder mixture composed of magnesium hydroxide and gibbsite using a planetary ball mill followed by its heating was conducted to prepare MgAl2O4 spinel. Both the starting materials are easily converted to amorphous phase by intensive grinding within 60 min. The monolithic MgAl2O4 spinel phase can be obtained from the mixtures ground over 15 min by calcination at 900 degreesC. The reactivity of the mixtures ground over 30 min is not improved. Prolonged finding promotes the aggregation of ground fine particles, but the aggregates deflocculate into fragments after calcination. (C) 2000 Elsevier Science B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据