4.7 Article

Polydimethylsiloxane thermal degradation - Part 1. Kinetic aspects

期刊

POLYMER
卷 42, 期 6, 页码 2395-2402

出版社

ELSEVIER SCI LTD
DOI: 10.1016/S0032-3861(00)00652-2

关键词

depolymerization of polysiloxanes; kinetics of depolymerization; thermal degradation

向作者/读者索取更多资源

A combination of traditional kinetic formal treatments and computer simulation has been made to analyze polydimethylsiloxane (PDMS) thermal degradation. It was shown that PDMS thermally decomposes to cyclic oligomers through Si-O bond scission in a chain-folded cyclic conformation energetically favored by overlapping of empty silicon d-orbitals with orbitals of oxygen and carbon atoms. Kinetic treatment shows that PDMS thermal volatilization, as rate of heating increases, becomes dominated by rate of diffusion and evaporation of oligomers produced on its decomposition. At high heating rate (e.g. 100 degreesC min(-1).) thermal decomposition in nitrogen and in air tend to overlap because the rate of reaction between the material and oxygen is strongly reduced by low-oxygen solubility and high-thermal degradation rate. In nitrogen a small black residue is formed (silicon oxycarbide) which is produced by an alternative decomposition path leading to cyclic oligomers, made possible at high heating rate. (C) 2000 Elsevier Science Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据