4.6 Article

Moisture and hydrogen-induced embrittlement of Fe3Al alloys

期刊

MATERIALS CHEMISTRY AND PHYSICS
卷 70, 期 2, 页码 236-241

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/S0254-0584(00)00482-X

关键词

environmental embrittlement; hydrogen microprint technique; iron aluminides

向作者/读者索取更多资源

Environmental embrittlement types of Fe3Al and Fe3Al-5Cr alloys have been evaluated using hydrogen microprint technique and tensile test in this study. The hot rolled iron aluminides offer better tensile strength and ductility in comparison to the as-cast iron aluminides in all test environments. Due to the fact that hydrogen transport in Fe3Al and Fe3Al-5Cr alloys is mainly lattice diffusion, the cleavage strength is decreased significantly by hydrogen. (C) 2001 Elsevier Science B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据