Studies of glycolysis of poly(ethylene terephthalate) recycled from postconsumer soft-drink bottles. I. Influences of glycolysis conditions

期刊

JOURNAL OF APPLIED POLYMER SCIENCE
卷 80, 期 7, 页码 943-948

出版社

JOHN WILEY & SONS INC
DOI: 10.1002/app.1174

关键词

glycolysis; poly(ethylene terephthalate); ethylene glycol; postconsumer soft-drink bottles; cobalt acetate; bis-2-hydroxyethyl terephthalate

向作者/读者索取更多资源

The glycolysis of recycled poly(ethylene terephthalate) flakes by ethylene glycol(EG) is investigated. Bis-2-hydroxyethyl terephthalate (BHET) and oligomers are predominately glycolysis products. The influences of glycolysis temperature, glycolysis time, and the amount of catalyst (cobalt acetate) are illustrated. The BHET, dimer, and oligomers are predominately glycolysis products. The optimum glycolysis temperature is found to be 190 degreesC. If a 190 degreesC glycolysis temperature, 1.5-h glycolysis time, and 0.002 mol glycolysis catalyst (cobalt acetate) are used, the glycolysis conversion is almost 100%. The glycolysis conversion rate increases significantly with the glycolysis temperature, glycolysis time, and the amount of cobalt acetate. Thermal analyses of glycolysis products are examined by differential scanning calorimetry. In addition, the chemical structures of glycolysis products are also determined by a Fourier transform IR spectrophotometer. (C) 2001 John Wiley & Sons, Inc.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据