block copolymer; amphiphilic; siloxane; living radical polymerization; copper

向作者/读者索取更多资源

Polydimethylsiloxane (PDMS) block copolymers were synthesized by using PDMS macroinitiators with copper-mediated living radical polymerization. Diamino PDMS led to initiators that gac-e ABA block copolymers, but there was low initiator efffciency and molecular weights are somewhat uncontrolled. The use of mono- and difunctional carbinol-hydroxyl functional initiators led to AB and ABA block copolymers with nar row polydispersity indices (PDIs) and controlled number-average molecular weights (M-n's). Polymerization with methyl methacrylate (MMA) and X-dimethyl aminoethyl methacrylate (DMAEMA) was discovered with a range of molecular weights produced. Polymerizations proceeded with excellent first-order kinetics indicative of living polymerization. ABA block copolymers with MMA were prepared with between 28 and 84 wt % poly(methyl methacrylate) with M-n's between 7.6 and 35 K (PDI <1.30), which show thermal transitions characteristic of block copolymers: ABA block copolymers with DMAEMA led to amphiphilic block copolymers with M-n's between 9.5 and 4.5.7 K (PDIs of 1.25-1.70), which formed aggregates in solution with a critical micelle concentration of 0.1 g dm(-3) as determined by pyrene fluorimetry experiments. Monocarbinol functional PDMS gave AB block copolymers with both MMA and DMAEMA. (C) 2001 John Wiley & Sons, Inc.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.2
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据