Effect of glass fiber and maleated ethylene-propylene rubber content on the impact fracture parameters of nylon 6

期刊

POLYMER
卷 42, 期 14, 页码 6161-6172

出版社

ELSEVIER SCI LTD
DOI: 10.1016/S0032-3861(01)00068-4

关键词

rubber toughened nylon 6; fiber reinforced; impact fracture parameters

向作者/读者索取更多资源

The impact fracture parameters of blends of nylon 6 and maleated ethylene-propylene rubber (EPR-g-MA) reinforced with glass fibers as a function of glass fiber and EPR-g-MA content were examined. Both the linear elastic fracture mechanics (LEFM) model and a modified essential work of fracture (EWF) model were used to analyze the data. It was found that the addition of EPR-g-MA to unreinforced nylon 6 increased the EWF parameters u(o) and u(d) defined by U/A = u(o) + u(d)l, where U/A is the total fracture energy per unit area and I is the ligament length. Beyond a critical rubber content, which coincided with the ductile-to-brittle transition, there was a large increase in u(d) When glass fiber reinforcement was used without rubber toughening, the EWF model was unable to model the observed fracture response. On the other hand, the LEFM model adequately described the fracture behavior, and it was found that the critical strain energy release rate, G(IC), increased with increasing glass fiber content. When both glass fiber reinforcement and rubber toughening were used, the u(o) increased with increasing EPR-g-MA or glass fiber content; whereas, u(d) increased with increasing ERR-g-MA content or decreasing glass fiber content. (C) 2001 Elsevier Science Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据