Photoelectrochemical study on the passive film on Fe

期刊

CORROSION SCIENCE
卷 43, 期 8, 页码 1403-1415

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/S0010-938X(00)00159-1

关键词

passive film; Fe; photocurrent; electronic properties; electronic transition; gamma-Fe2O3

向作者/读者索取更多资源

Electronic properties of the passive film formed on Fe in pH 8.5 buffer solution were examined by the photoelectrochemical spectroscopy. Photocurrent responses for the passive film on Fe with film formation potential are explained by the modified band structure model developed on the basis of that for crystalline spinel (gamma -Fe2O3) involving two types of electronic excitation processes, i.e., the p-d and the d-d transition. The photocurrent spectra for the passive film on Fe measured in a wide range of photon energy could be resolved into two components of photocurrent spectrum reflecting effects of each electronic transition on the photocurrent spectra. The band gap energy of each electronic transition process was determined from the resolved photocurrent spectrum; 2.87 eV for the d-d transition, and 3.67 eV for the pd transition. A small photocurrent peak at 2.7 eV appeared at film formation potentials higher than 400 mV was associated with the formation of gamma -FeOOH layer on gamma -Fe2O3 him. (C) 2001 Published by Elsevier Science Ltd.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据