Hydrogen evolution on NiPx alloys:: the influence of sorbed hydrogen

期刊

INTERNATIONAL JOURNAL OF HYDROGEN ENERGY
卷 26, 期 11, 页码 1193-1198

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/S0360-3199(01)00053-2

关键词

hydrogen evolution; Ni-P alloys; electrodeposition; adsorption

向作者/读者索取更多资源

NiPx alloys were formed by electro deposition. P content in the range from 10 to 27 at% was obtained by altering the deposition current and the composition of the deposition electrolyte. For all the alloys the hydrogen evolution was measured in an alkaline solution. The catalytic activity of the alloys varied with several decades. The maximum activity was obtained for a Ni alloy with 12 at% P. The amount of hydrogen adsorbed to the surface and absorbed into the NiPx alloys was measured. The highest catalytic activity was obtained for the alloys that sorbed a large amount of hydrogen. For the hydrogen reaction a Tafel slope close to 60 mV/dec was observed, The measurement of adsorption isotherms showed the Frumkin isotherm to give the best fit of the data. This isotherm also provided an explanation for the Tafel slopes. (C) 2001 Elsevier Science Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据