Low T oxidation followed by brief sonication in hot HCl has been optimized to remove Fe catalyst residues from HiPco material with minimal loss of tubes. One pass reduces Fe from 6-10 to 0.6-1.6 at.% with 60% yield, most of the loss being Fe. Raman scattering reveals a broad diameter distribution with a mean of 1.0-1.1 tun. After purification we find excellent correlation between oxidation temperature and Raman spectra whereby the oxidation rate varies inversely with tube diameter. This can be explained by the larger strain associated with greater curvature of small tubes. (C) 2001 Elsevier Science B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据